We use first- and third-party cookies including other tracking technologies from third party publishers to give you the full functionality of our website, to customize your user experience, perform analytics and deliver personalized advertising on our websites, apps and newsletters across internet and via social media platforms. For that purpose, we collect information about user, browsing patterns and device.

By clicking "Accept All Cookies", you accept this, and agree that we share this information with third parties, such as our advertising partners. If you prefer, you can choose to continue with "Only Required Cookies". But keep in mind that blocking some types of cookies may impact how we can deliver tailored content that you might like.

For more information and to customize your options, click on "Cookie settings". If you want to learn more about cookies and why we use them, visit our Cookie Policy page at any time. Cookie Policy

Accept All Cookies Close
BB-2232 Phenolic Edge Protection Resin

BB-2232 Phenolic Edge Protection Resin

Product Description

BB-2232 is glass fiber filled Phenolic with black grit appearance.

Product Details

Features

Features: Extreme hardness, very good grinding and polishing properties, does not stick on embedding instruments,non adherent.
Application: All hard materials, e.g. hardened gears, hard metals and ceramics.

Technical Parameters

Description

Glass fiber filled Phenolic

Components

black grit

Heat time

4-6 min

Cooling time

2-3 min

Pressure

High/Medium

Pressure

100-150 bar

Heat temperature

140-180 °C

Hardness

90-93 (Shore D)

 

Ordering Information

Order No:

Description

Package

02.01.210

Black, Glass fiber filled, Grit

1 kg

02.01.220

Black, Glass fiber filled, Grit

4 kg

02.01.225

Black, Glass fiber filled, Grit

20 kg



Our Advantage

  • High Quality

    Our production capacity can meet the needs of different customers with different purchase quantities.
  • Preferential price

    As a professional China Custom BB-2232 Phenolic Edge Protection Resin Manufacturers, We have our own equipment, one-stop production, factory direct sales, high quality and low price.
  • Custom service

    We have a strong and production team, which can develop and produce custom BB-2232 Phenolic Edge Protection Resin according to the product description or sample provided by customers.
  • Rich products

    It can meet the development and production of many different industries.

Contact Us

Recommended