TJ 2227 Epoxy Resin (2:1)
Product Description
Epoxy Curing System is typically used for excellent flow and penetration, or when better adhesion, chemiacl resistance, less shrinkage and clarity are required.
We use first- and third-party cookies including other tracking technologies from third party publishers to give you the full functionality of our website, to customize your user experience, perform analytics and deliver personalized advertising on our websites, apps and newsletters across internet and via social media platforms. For that purpose, we collect information about user, browsing patterns and device.
By clicking "Accept All Cookies", you accept this, and agree that we share this information with third parties, such as our advertising partners. If you prefer, you can choose to continue with "Only Required Cookies". But keep in mind that blocking some types of cookies may impact how we can deliver tailored content that you might like.
For more information and to customize your options, click on "Cookie settings". If you want to learn more about cookies and why we use them, visit our Cookie Policy page at any time. Cookie Policy
Product Description
Epoxy Curing System is typically used for excellent flow and penetration, or when better adhesion, chemiacl resistance, less shrinkage and clarity are required.
Features
Colorless and transparent, electrically conductive, suitable for SEM analysis.
Technical Parameters
Part A |
Liquid |
Part B |
Liquid |
A : B ( w/w ) |
2 : 1 |
Pot life |
5-10min @100g |
Cure time (22-25˚C) |
2-4h |
Peak temperature |
92°C |
Hardness |
80 D |
Edge protection |
Good |
Ordering Information
Order No: |
Description |
Package |
02.04.920 |
Epoxy Resin, Liquid |
1 kg |
02.04.921 |
Epoxy Curingagent, Liquid |
0.5 kg |
Similar Products
Trojan |
Struers |
Buehler |
ATM |
TJ 2562A |
EpoFix |
EpoThin 2 |
x |